Practice Free NACE-CIP1-001 Exam Online Questions
Stripe coats are generally applied to:
- A . Edges and corners
- B . Welds
- C . Complex geometric shapes
- D . a), b), and c)
You ate the NACE Inspector on a job where NACE No. 2/SSPC – SP 10 has been specified. You are finding the Contractor is leaving mill scale on the on surface and as a result you have been rejecting the blast. The Contractor is very upset and has told you that the standard permits up to 5% of the mill scale to remain and still be in be in compliance with the standard.
Your FIRST preferred course of action is to:
- A . Review the relevant standard with the Contractor
- B . Permit coating to take place so as not to lose the blast
- C . Call your supervisor
- D . Shut the job down
In a non-convertible coating the role of the primary solvent is to:
- A . To make the coating flow out better
- B . To dissolve the resin
- C . To promote faster cure
- D . To control the evaporation rate
Check abrasive blast pressure with a
- A . needle pressure gauge
- B . replica tape
- C . surface comparator
- D . nozzle aperature gauge
Whenever dissimilar metals must join, the most common practice is to
- A . provide cathodic protection to prevent corrosion,
- B . provide anodic protection to prevent corrosion.
- C . coat all connected dissimilar metals.
- D . avoid coating all connected dissimilar metals.
According to SSPC PA 2 a Spot Measurement is:
- A . A single gauge reading
- B . The average of gauge readings taken in a 4cm (1.5 inch) circle
- C . The overall average of all readings
- D . The average of all spot measurements in a given area
The form of corrosion that has the largest potential for unexpected catastrophic failure is:
- A . General Corrosion
- B . Atmospheric Corrosion
- C . Galvanic Corrosion
- D . Localized Corrosion
Checking is
- A . an exposed area of the substrate or previous coat material, caused by poor application technique.
- B . a fine crack in the surface of a coating that rarely reaches the substrate
- C . a very small hole in a coating caused when air or solvent is trapped in porous film and then escapes.
- D . surface breaks in the film that often result from grease or oil contamination and revel the substrate.
The most important factor resulting in improved job site safety is:
- A . Personal Protective Equipment
- B . Engineering Controls
- C . Safety Enforcement
- D . Situational Awareness
If the project specification DOES NOT state the specific DFT measurement standards, the inspector should use
- A . a recognized industry standard like SSPC-PA 2 that is broadly accepted